Shenzhen ZYH Hardware and Plastic Products Co., Ltd. +86 189 2939 4378 nickcopy698@gmail.com

Oct 16, 2026 · BLOG

Ribs and corner radius

Crate corners take the impact in daily logistics. A radius that is too small concentrates stress and cracks after a few hundred trips; we size the radius against wall thickness and load.

Draft angle

Every vertical wall needs enough draft to release without scuffing. Textured surfaces need 1–1.5° extra, which is often forgotten when a customer supplies a drawing made for a smooth part.

Gate position

Gates are placed where the flow front meets last, so weld lines land on a non-critical rib rather than a visible side wall or a hinge.

Cooling, ejection and trial

Balanced cooling and enough ejector area prevent warping; then T1 samples are dimensionally reported before the tool is accepted.

← Back to Mold Knowledge